Main characteristics
Properties |
Units |
Results |
Limits |
Methods |
Appearance |
- |
conform |
limpid |
Visual |
|
|
|
homogeneous |
examination |
Density at 20oC |
kg/dm3 |
0.866 |
max 0.875 |
ASTM D 4052 |
Kinematic viscosity at |
|
|
|
ASTM D 445 |
50oC |
mm2/s |
8.94 |
min 8.00 |
|
-40oC |
|
3489 |
max 4000 |
|
Acid number |
mg KOH/g |
0.02 |
max 0.10 |
ASTM D 974 |
Flash point, closed cup |
oC |
150 |
min 145 |
ASTM D 93 |
Pour point |
oc |
-57 |
max -55 |
ASTM D 97 |
Foaming test at 24oC |
ml/ml |
30/0 |
max 100/0 |
ASTM D 892 |
Thermooxidative stability |
|
|
|
GOST 23797-79 |
50 hat 150 oC |
|
|
|
|
after test: |
|
|
|
|
a / Total acid number |
mg KOH/g |
0.08 |
max 0.40 |
|
b/ Viscosity at |
|
|
|
|
+50 oC |
mm2/s |
9.14 |
max 10.0 |
|
-40 oC |
|
4099 |
max 5500 |
|
c/ Corrosion |
|
|
|
|
Steel SHKH-15 |
mg/cm2 |
0.0 |
0.0 |
|
Aluminium AK-4 |
|
0.0 |
0.0 |
|
Copper |
|
0.00 |
max.+/-0.20 |
|
c/Isooctan insoluble |
%by weight |
0.03 |
max 0.10 |
|
Antiwear additive content |
% by weight |
1.2 |
1.1-1.3 |
FTIR |
Related goods and services